Another batch is drying.

So easy to make.

Grade 5 titanium and PA6-CF plus some 1.5 mm stainless rods.

you are viewing a single comment's thread
view the rest of the comments
[–] aceofspades 2 points 2 months ago (6 children)

What do you make your levers out of?

[–] mossyspook@fosscad.io 1 points 2 months ago (5 children)

I'm experimenting with both PLA+ and PA6-CF

I had a PLA+ one last 450 rounds before it got too hot and warped.

Havent gotten enough testing on the CF one yet.

[–] TheShittinator 2 points 2 months ago (4 children)

o/ Hi, sorry to bug you: could you reply to this comment? I'm testing a thing and want to make sure I haven't broken federation.

[–] TheShittinator@fosscad.io 1 points 2 months ago (1 children)

Nevermind, I can just do this from the other end via my own account lol

[–] TheShittinator 2 points 2 months ago
load more comments (2 replies)
load more comments (2 replies)
load more comments (2 replies)